王国新, 许玉宇, 王慧, 刘烽, 吴骋, 胡清. 电感耦合等离子体发射光谱法测定红土镍矿中镍钴铜[J]. 岩矿测试, 2011, 30(5): 572-575.
引用本文: 王国新, 许玉宇, 王慧, 刘烽, 吴骋, 胡清. 电感耦合等离子体发射光谱法测定红土镍矿中镍钴铜[J]. 岩矿测试, 2011, 30(5): 572-575.
WANG Guo-xin, XU Yu-yu, WANG Hui, LIU Feng, WU Cheng, HU Qing. Determination of Ni, Co and Cu in Laterite-Nickel Ores by Inductively Coupled Plasma-Atomic Emission Spectrometry[J]. Rock and Mineral Analysis, 2011, 30(5): 572-575.
Citation: WANG Guo-xin, XU Yu-yu, WANG Hui, LIU Feng, WU Cheng, HU Qing. Determination of Ni, Co and Cu in Laterite-Nickel Ores by Inductively Coupled Plasma-Atomic Emission Spectrometry[J]. Rock and Mineral Analysis, 2011, 30(5): 572-575.

电感耦合等离子体发射光谱法测定红土镍矿中镍钴铜

Determination of Ni, Co and Cu in Laterite-Nickel Ores by Inductively Coupled Plasma-Atomic Emission Spectrometry

  • 摘要: 红土镍矿样品用无水Na2CO3-Na2B4O7混合熔剂熔融,HCl浸出酸化,电感耦合等离子体发射光谱法直接测定样品中镍、钴、铜的含量。Cu 324.754 nm使用Y 371.030 nm作为内标线,Ni 231.604 nm、Co 228.616 nm使用Y 224.306 nm作为内标线校正基体干扰,方法检出限镍为0.5 μg/g、钴为1.0 μg/g、铜为1.0 μg/g,相对标准偏差(RSD,n=7)为1.2%~2.0%,加标回收率为95.0%~103.6%,能满足红土镍矿的分析要求。

     

    Abstract: A method for the determination of Ni, Co and Cu contents in laterite is presented in this paper. Laterite samples were fused with a mixed flux of Na2CO3-Na2B4O7, then the analytes were extracted by HCl acid. The sample solution was measured by inductively coupled plasma-atomic emission spectrometry (ICP-AES). The internal standard method was used to avoid matrix interference based on choosing Y 371.030 nm as the internal calibration line for Cu (324.754 nm) and Y 224.306 nm for Ni (231.604 nm) and Co (228.616 nm). The detection limits for Ni, Co and Cu were 0.5 μg/g, 1.0 μg/g and 1.0 μg/g, respectively. The relative standard deviations (RSD) of the test result were 1.2%-2.0% (n=7), and the recoveries ranged from 95% to 103.6%, which met the requirements of analysis for laterite.

     

/